Natural Hemostatic Function of Collagen

Damage to the blood vessel wall leads to subendothelial collagen release. The collagen directly or indirectly interacts with the surface receptors on thrombocytes. The binding of collagen initiates a reaction cascade leading to transformation and aggregation of the thrombocytes. Additionally, the thrombocytes are cross-linked by fibrinogen. The resulting (white) thrombus initially stabilizes the wound. Accordingly, collagen sponges support the formation of a blood coagulum and contribute to a rapid stabilization of the wound area. Due to their hemostatic effect, collagen sponges and cones can be used for stabilization of biopsy harvesting sites or covering of minor oral wounds and extraction sockets, respectively.

Safe and Natural Product

collacone® is produced of porcine dermis by a standardized, controlled purification process. The dermis is carefully cleaned by several wet-chemical purification steps, lyophilized and sterilized by gamma irradiation. The unique production process guarantees a safe end-product, free from cells and chemical residues.

Collagen is a highly versatile material that, due to its low immunogenicity and superior biocompatibility and that of the degraded end-products, is widely employed in biomedical and pharmacological applications 6. The natural hemostatic function of the collagen together with its complete degradation make collacone® an ideal product to apply in fresh extraction sockets, to cover wounds, helping control the bleeding and stabilizing the wound.

Safe and Sterile

After a thorough analysis of the donors’ medical history, the high safety of maxgraft® is ensured by a series of stringent serological tests in combination with C+TBA’s Allotec® purification process and final radiological sterilization.

C+TBA is certified as a tissue procurement facility and tissue bank according to §19 and §22 of the Austrian Tissue Safety Act.

Origin

maxgraft® is processed allograft from human donors. All cancellous blocks originate from femoral heads of living donors donated during hip arthroplasty surgery. Uni-cortical blocks with a cortical component are from post-mortem donors. Procurement is standardized according to a predefined protocol and is performed by certified procurement centers. All tissue donations are performed only after the donor has given written consent. In addition, the health status of each potential donor is assessed in advance as part of a risk analysis and the donor is then selected on the basis of strict exclusion criteria.

Rehydration

maxgraft® blocks consist of a mineralized collagen matrix with a residual moisture content of <10%. Nevertheless, rehydration is recommended (10 minutes in physiological saline solution). maxgraft® blocks can also be briefly rehydrated in a disposable syringe under vacuum in physiological saline solution (technique according to Dr. Blume). Rehydration can improve the adaptability of the material (especially with large blocks) to the defect.

Variants Depending on Clinical Situations

maxgraft® blocks are available in pure cancellous and uni-cortical forms. For the regeneration of bone defects, the cancellous structure of the purely cancellous blocks enables rapid regeneration of vital bone tissue, whereas the uni-cortical blocks offer more volume stability, for example in augmentations outside the ridge contour.

Advantages of Maxresorb® Compared to Xenogeneic Bone Substitutes

• maxresorb® is a 100% synthetic, thus very safe biomaterial (not even theoretical risk of disease transmission with regard to raw material)
• Its use is not restricted by dietary or religious conflicts
• Valid synthetic alternative to xenografts with regards to indications and handling
• Composition and structure of synthetic bone grafts can be designed to obtain optimal material characteristics:
  – The micro-/macrostructure of maxresorb® is rationally designed to provide the ideal properties of a bone substitute, naming high porosity, interconnected pores and very rough, hydrophilic surface
– Owing to its synthetic, biphasic composition, maxresorb® is characterized by a controlled resorption and full remodeling potential. After about 2-3 years the material will be replaced by patients’ own bone

Controlled Full Resorption of Maxresorb®

In particular, pure ß-TCP resorbs very rapidly, i.e. within a few weeks from the initial insertion. In contrast, pure synthetic HA is characterized by a very slow resorption and sometimes soft tissue encapsulation. Thus, the combination of HA and ß-TCP in maxresorb® offers the advantages of both materials, with a final biomaterial that shows excellent osteoconductivity. While the fast resorption of β-TCP (within about 3 months) quickly offers space for new bone formation, the HA component provides volume stability for an extended time period (resorption within 2-3 years).

Controlled Remodeling of Maxresorb®

maxresorb® exhibits a controlled remodeling within about 2 to 3 years. Following implantation, the particles are first integrated into the forming bone, but then are gradually resorbed and remodeled. The β-TCP component remodels within 3-6 months while the HA component resorbs much slower within >2 years.

Maxresorb: The Ideal Mix of Hydroxyapatite (HA) and Beta-Tricalcium Phosphate (Β-TCP)

An ideal bone regeneration material should be slowly resorbed while new bone matrix is formed. The basic principle of maxresorb® and, more in general, of biphasic calcium phosphates, is to achieve a balance between the properties of hydroxyapatite (HA) and beta-tricalcium phosphate (β-TCP). Pure β-TCP resorbs quite fast due to high solubility and therefore, may not offer sufficient volume stability for larger augmentative procedures. On the other hand, pure synthetic HA resorbs very slowly and some studies have demonstrated the inferior osteoconductivity of synthetically produced HA when used alone. By mixing HA and β-TCP the advantages of both materials are combined to achieve a material with good osteoconductive as well as resorption properties 8. Studies have shown that the optimal HA/ β-TCP ratio lies between 65:35 and 55:45 1, 2, 9. Therefore, maxresorb® with its biphasic composition of 60% HA and 40% β-TCP offers and optimal balance between resorption and stability. Bone regeneration materials based on mixtures of HA and β-TCP have been successfully applied in dental regenerative surgery for more than 20 years.